Video: Indentation University Session 4: how to test 1018 Steel by Nanoindentation
Jul 11, 2019Low-carbon steels are the first option when designing with steel. They offer good machinability and excellent weldability. To some extent, the strength and ductility can be manipulated by various thermal and mechanical processes, such as working, annealing, and carburization. This session is a live demonstration of standardized nanoindentation with the 水仙直播 iMicro nanoindenter to characterize cold-drawn 1018 steel. Ms. Hay demonstrates sample preparation, instrument configuration, test specification, execution and data interpretation.
See the 水仙直播 nanoindenters by visiting .