水仙直播

Session 12 – How to Test Low-k Thin Films by Nanoindentation

Mar 12, 2020

In digital circuits, materials with low permittivity separate the conducting parts from one another; materials with lower permittivity provide better electrical and magnetic insulation. Continuous reduction in scale drives the optimization problem of lowering the permittivity of the insulator as much as possible, without compromising mechanical integrity, as quantified by the Young’s modulus. (The dielectric constant, k, is a dimensionless expression of permittivity, having been normalized by vacuum permittivity.)

This session is a live demonstration of the nanoindentation technique for measuring the Young’s modulus of a blanket low-k film on silicon using the 水仙直播 iNano platform. Ms. Hay demonstrates sample preparation, instrument configuration, test specification, and data interpretation, including proper accounting of substrate influence.

Are you sure?

You've selected to view this site translated by Google Translate.
水仙直播 China has the same content with improved translations.

Would you like to visit 水仙直播 China instead?


您已选择查看由骋辞辞驳濒别翻译翻译的此网站。
碍尝础中国的内容与英文网站相同并改进了翻译。

你想访问碍尝础中国吗?

If you are a current 水仙直播 Employee, please apply through the 水仙直播 Intranet on My Access.

Exit

This site is registered on as a development site. Switch to a production site key to .